Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c7ad58d3c0b071069a8ee0cb8c8ba2e8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F2800-20 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F8-14 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-44 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F222-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D133-04 |
filingDate |
1995-04-19^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
1996-05-14^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9d8daaaf801b1207b969660983acd534 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_53b16ebfbf8b1022f6adaefa33c2b2de http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_399669e31333a7a14768bcfeae7f445e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fad8c353f7cf2ad1221444f2fb89be7b |
publicationDate |
1996-05-14^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-5516853-A |
titleOfInvention |
Process for the production of water-dilutable binders and their use in coating compositions |
abstract |
The present invention relates to a process for the production of oxidatively crosslinkable, water-dilutable binders by a) forming a copolymer having intramolecular carboxylic anhydride groups by copolymerizing anhydride-functional compounds, other olefinically unsaturated monomers and 5 to 50% by weight, based on the weight of the olefinically unsaturated monomers used for the production of the copolymers a), of monomers which cannot be homopolymerized under the reaction conditions, b) subsequently reacting by ring-opening esterification at least 50% of the anhydride groups present in the copolymer with one or more unsaturated monohydric alcohols, c) reacting by ring-opening esterification up to 50% of the anhydride groups with monohydric saturated alcohols having a molecular weight of 32 to 200 either before, during or after step b), d) optionally reacting 1 to 70% of the carboxyl groups formed in steps b) and c) with organic epoxide compounds and e) neutralizing at least a portion of the carboxyl groups formed in steps b) and c). The present invention also relates to the binders obtained by this process and to their use in water-dilutable lacquers and coating compositions. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010197878-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5773518-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5948843-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-5811481-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7071260-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2006229375-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2010168362-A1 |
priorityDate |
1994-04-29^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |