Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29L2007-008 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2201-068 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2201-0141 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-1105 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K1-0393 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29K2105-0079 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K2203-0152 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H05K3-0011 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K1-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C71-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H05K3-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 |
filingDate |
2004-09-23^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2010-06-22^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c42871432c98e590e19b2e9ecc3d6514 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68089d393f6b47981b0d4d0b6bba08c9 |
publicationDate |
2010-06-22^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-7740790-B2 |
titleOfInvention |
Method of making liquid crystal polymer films |
abstract |
A method of making a thermotropic liquid crystal polymer film includes continuously heat treating of the thermotropic liquid crystal polymer film 2 while the latter is jointed to a sheet-like support member 4 , and subsequently separating the heat-treated thermotropic liquid crystal polymer film 2 from the support member 4 . The continuous heat treatment of the thermotropic liquid crystal polymer film 2 then jointed to the support member 4 is carried out for a predetermined heating time within the range of 5 to 60 seconds at a predetermined heating temperature T° C. equal to or higher than the melting point Tm° C. of the thermotropic liquid crystal polymer film less 15° C. (i.e., Tm−15° C.), but lower than the melting point Tm° C. (thus, Tm−15° C.≦T° C.<Tm° C.), to thereby increase the thermal expansion coefficient of the thermotropic liquid crystal polymer film. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9538646-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8557552-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9822306-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/TW-I616328-B http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9439303-B2 |
priorityDate |
2003-09-30^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |