http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7993707-B2
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_95c89084d61fd47ae93470ca7c96f184 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C09D183-04 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D3-02 |
filingDate | 2006-08-10^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate | 2011-08-09^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2a15d9efbf4835d76f307812f5a675e9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_082de9b40985beb489407477578da25a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8eb4bb4d4c009ed25e8535e67b107c40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_485f21ebbaca8f64d9b913a6afb904c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8b32cda835f9e4093693cdd4167f53d3 |
publicationDate | 2011-08-09^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | US-7993707-B2 |
titleOfInvention | Production of coated substrates |
abstract | The present invention relates to a process for coating substrates, which comprises the steps:n a) provision of a substrate, b) application of a composition to at least one surface of the substrate, the composition comprising a silane of the general formula (Z 1 )Si(OR 3 ), where Z 1 is OR or Gly (Gly=3-glycidyloxypropyl) and R is an alkyl radical having from 1 to 6 carbon atoms and all radicals R can be identical or different, an inert solvent and an initiator and the inert solvent having a boiling point under the drying conditions of step c) which is in a range from 50° C. above to 50° C. below the drying temperature of step c) and the boiling point of the inert solvent under the drying conditions of step c) being at least 80° C., and c) drying of the composition applied in step b) at a drying temperature of from 100° C. to 250° C.,n nand also to a coated substrate obtainable by means of the abovementioned process. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017233607-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2013004137-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9535215-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10316217-B2 |
priorityDate | 2005-11-03^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links