Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2b3480c462296b82923a6edef071d8ba http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0a20f7bb153b6c859eefb170a469ebf0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_01bdf8c781b3306beec9517bb11479f8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M2300-0082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J2371-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-50 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08J5-2256 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-0289 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1025 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1032 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/H01M8-1011 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01M8-00 |
filingDate |
2007-05-07^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2012-07-10^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fc03053a80f419c7fb219f44f8fc0e24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2e5dd8a0011059ed590cd5b083ab759c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_19a24d6a03c0936d4be6678c1d1a9c22 |
publicationDate |
2012-07-10^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8216727-B2 |
titleOfInvention |
Aromatic hydrocarbon based proton exchange membrane and direct methanol fuel cell using same |
abstract |
A proton exchange membrane is obtained which can give an excellent power generation characteristic when the membrane is applied to, in particular, a fuel cell wherein high-concentration methanol is used as a fuel. In the aromatic hydrocarbon based proton exchange membrane of the invention, the ion exchange capacity is set into the range of 0.6 to 1.3 meq/g. Moreover, the area swelling rate for a 30% by mass methanol aqueous solution at 40° C. is set into the range of 2 to 30%. Preferably, a sulfonic acid group is bonded to an aromatic ring of the aromatic hydrocarbon based polymer contained in the aromatic hydrocarbon based proton exchange film. Preferably, the aromatic hydrocarbon based polymer is a polyarylene ether based polymer. |