abstract |
A thermoplastic polymer material containing starch is shown and described, which can be obtained by homogenizing a mixture containing 40 to 85 wt.-% starch and/or starch derivative, 15 to 55 wt.-% softener, and 0.01 to 7 wt.-% of a polymer which contains an epoxy group, while supplying thermal and/or mechanical energy and setting the water content of the mixture to less than approximately 12 wt.-%. The polymer material according to the invention is characterized by outstanding mechanical properties. |