Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8e071d18fea054bf8d1420d483e78ed1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_aff738df55c6c06d4cb497c95dca35e5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_83c363840c383ad4fe17ba184ec205a7 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03F7-0002 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B29C39-026 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/B82Y40-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03F7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C7-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C39-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B82Y40-00 |
filingDate |
2009-06-26^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2014-09-16^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fc55a268ec4c3882c40612aa68c1ee7 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b8fe3d1e145ba3163634d8f296cd7bb6 |
publicationDate |
2014-09-16^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-8833430-B2 |
titleOfInvention |
Versatile high aspect ratio actuatable nanostructured materials through replication |
abstract |
A method of forming a nanostructured surface, including providing an original nanostructured surface having an array of high aspect ratio structures formed on a planar substrate; forming a negative replica mold of the original nanostructured surface, where the negative replica mold includes a flexible material; deforming the negative replica mold; and using the deformed negative replica mold to form a deformed replica of the original nanostructured surface, where the deforming step is performed at least one of before, during, or after introducing a material for forming the deformed replica into the negative replica mold. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10062831-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11441051-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2017040524-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3988282-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-3456506-A4 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11104043-B2 |
priorityDate |
2008-06-26^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |