Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_129e393582e6bdf4029baf2206522f45 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-325 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K2003-324 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L2205-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L101-16 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08G63-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K3-32 |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-16 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-06 |
filingDate |
2013-09-12^^<http://www.w3.org/2001/XMLSchema#date> |
grantDate |
2018-03-20^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_eb6337401feb1ba743fe2d9657a3dae0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7cd03a7372e5d99a80941a1d0113097b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a42ec38590a79e4c320a91a70ea8a44e http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b0f4517551a95b78a5795d0e87a6490 |
publicationDate |
2018-03-20^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
US-9920181-B2 |
titleOfInvention |
Polylactic acid resin composition, molded product, and method of manufacturing polylactic acid resin composition |
abstract |
A polylactic acid resin composition includes: 0.005 parts by weight to 1.2 parts by weight of a metal phosphate represented by Formula (1):n nM x H y PO z (1)n n(in Formula (1), M is an alkali metal atom or an alkaline earth metal atom, and x, y, and z are integers satisfying 1≦x≦2, 1≦y≦4, and 2≦z≦8, respectively) with respect to 100 parts by weight of a polylactic acid resin including a poly-L-lactic acid component and a poly-D-lactic acid component, wherein a crystallization enthalpy of crystals in the polylactic acid resin is not less than 5 J/g when a temperature of the polylactic acid resin composition is increased to 250° C., and the temperature is kept constant for 3 minutes, followed by decreasing the temperature at a cooling rate of 20° C./min in differential scanning calorimetry. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-11643261-B2 |
priorityDate |
2012-10-10^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |