abstract |
The present invention relates to a resin mixture comprising: a first resin; and a second resin having a hydrophobic functional group in a side chain thereof and having a surface energy difference of 0.1 to 20 mN/m between the first resin and the second resin at the temperature of 25˚C, the resin mixture being capable of forming a layer separation structure. The present invention also relates to a pellet, a method for manufacturing the same and a resin molding product having a specific layer separation structure. The resin mixture of the present invention may not only improve mechanical properties and surface hardness of the molding product but also shorten process time, increase productivity and reduce production cost by omitting an additional surface coating step. |