http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-9300368-A1
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_fc307b3aeede7c7f137de525de9b8498 |
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-6578 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-6565 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08F4-6567 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E03C1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A47K3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-645 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F10-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05B3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05B1-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05B1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05B1-16 |
filingDate | 1992-06-19^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a632ab91463d4754dad92269ca20c6c9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_81a9ec7394e3cc4da30d48334a859481 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_642b8a702a3c3825dac903355a04f129 |
publicationDate | 1993-01-07^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | WO-9300368-A1 |
titleOfInvention | Supported high activity polyolefin catalyst component with regular distribution of magnesium values provided utilizing a controlled drying protocol |
abstract | A novel catalyst support and a method for preparation thereof, characterized by the presence of selected amounts of a hydrocarbon soluble magnesium-containing compound applied to the support relative to solvent, wherein a surface uniformly and essentially continuously moistened with the solvated magnesium compound is achieved in a condition of incipient precipitation to permit the formation of a regular essentially continuous distribution of the magnesium compound onto and conforming to the support material. The drying process under these conditions is effective in maintaining to a high degree the effective surface area and pore volume of the material. The support containing the adsorbed magnesium in then dried in a controlled manner to essential incipient wetness conditions providing a regular spatial distribution of stacked reticular magnesium values at a level of one to five molecular monolayers on the support. A representative process for polymerizing or copolymerizing olefins providing stereospecific polymers such as propylene is disclosed. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-100371476-B1 |
priorityDate | 1991-06-20^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links